Alloy 28 and 904L are not interchangeable grades. Both are high-alloy austenitic materials used in corrosive process equipment, but Alloy 28 (UNS N08028) contains substantially more chromium and nickel, while 904L (UNS N08904) contains more molybdenum in typical producer data. The better choice depends on the exact acid, concentration, temperature, chlorides, contaminants, product form and governing specification—not on a single “corrosion-resistant” label.
Alloy 28 vs 904L at a Glance
| Selection factor | Alloy 28 / UNS N08028 | 904L / UNS N08904 |
|---|---|---|
| Material family | High-alloy austenitic Fe-Ni-Cr-Mo-Cu material | High-alloy low-carbon austenitic stainless steel |
| Common designations | UNS N08028, EN 1.4563, X1NiCrMoCu31-27-4 | UNS N08904, EN 1.4539, 904L |
| Typical chemistry emphasis | Higher chromium and nickel; Mo and Cu additions | High Ni and Mo with Cu addition and low carbon |
| Typical application focus | Phosphoric acid, sour oil and gas, chloride-bearing chemical service, refinery equipment | Sulfuric-acid handling, chemical and petrochemical equipment, flue-gas cleaning, seawater and desalination equipment |
| Procurement warning | Confirm the product standard and availability for the requested form | Do not substitute for Alloy 28 solely because both are austenitic and copper-bearing |
Chemistry and performance descriptions are selection guidance. Purchase acceptance must follow the specified standard, ordered condition and actual MTC.
Composition: Why the Grades Behave Differently
Producer data for Sanicro 28 lists a nominal composition around 27% chromium, 31% nickel, 3.5% molybdenum and 1.0% copper. Outokumpu lists typical 904L chemistry around 19.8% chromium, 24.2% nickel, 4.3% molybdenum and 1.4% copper. These values explain why the two grades should not be treated as equivalents.
- Chromium supports passivation and resistance in oxidizing conditions. Alloy 28 has the higher nominal chromium level in these producer datasets.
- Nickel helps maintain the austenitic structure and improves resistance in several reducing and stress-corrosion conditions. Alloy 28 has the higher nominal nickel level.
- Molybdenum supports resistance to localized attack and reducing media. 904L has the higher typical Mo value in the cited Outokumpu data, but chemistry alone does not predict performance in every process stream.
- Copper contributes to performance in sulfuric-acid service. Both grades contain copper.
These are typical producer values, not universal acceptance limits. A purchase order should specify the UNS number and governing material standard; the supplied heat must be checked against its Mill Test Certificate.
Corrosion Selection by Service Environment
Phosphoric acid and fertilizer processing
Alloy 28 was developed for demanding phosphoric-acid processing and is used where chlorides and process contaminants make service more severe. Alleima reports strong performance for Sanicro 28 in highly aggressive phosphoric-acid environments. This makes Alloy 28 a serious candidate for heat exchangers, piping, pumps, valves and machined parts in wet-process acid plants. The actual acid concentration, temperature and impurity profile must still be reviewed.
Sulfuric acid and general chemical processing
904L was developed for sulfuric-acid service and remains widely specified for chemical and petrochemical equipment. It can be an economical and well-established option where corrosion data, fabrication practice and the applicable code support it. Alloy 28 may also perform well in sulfuric-acid and mixed-acid conditions, but it should not be selected merely because it contains more nickel and chromium.
Chlorides, seawater and localized corrosion
Both grades are used beyond conventional stainless steels in chloride-bearing service. Alloy 28 is characterized by high resistance to pitting, crevice corrosion and stress-corrosion cracking in several chloride-containing environments. 904L offers very high general corrosion resistance and is used in seawater handling and desalination, but seawater duty is not one uniform condition. Temperature, flow, deposits, crevices, oxidants and biological activity can change the result.
Sour oil and gas service
Alloy 28 is widely used in hydrogen-sulfide-containing environments, including production tubing and refinery heat exchangers. For sour service, material selection must also comply with the project’s applicable sour-service requirements, hardness limits, heat treatment, manufacturing route and qualification records.
Product Standards and Forms
| Product form | Alloy 28 reference | 904L reference |
|---|---|---|
| Bar and rod | EN 10088-3 / EN 10272 are listed by Alleima for Sanicro 28 bar. Do not assume ASTM B473 covers N08028. | ASTM A479/A479M with A484/A484M for applicable bar orders; EN 10088-3 / EN 10272 may apply to European procurement |
| Seamless pipe and tube | ASTM B668 | ASTM A312/A312M for pipe; ASTM A269/A269M for general-service tubing, subject to the ordered edition and application |
| Welded pipe / tube | Confirm the required project standard and approved manufacturing route | ASTM A312/A312M for welded pipe; ASTM A249/A249M or A269/A269M may apply to tube depending on service |
| Plate and sheet | ASTM B709 | ASTM A240/A240M |
The same UNS grade can be supplied under different standards depending on product form. A pipe standard cannot be used as the acceptance basis for bar simply because the chemistry designation is the same.
How to Choose: A Practical Engineering Sequence
- Define the process stream: identify every acid, chloride, oxidant, reducing species, H₂S and contaminant.
- State concentration and temperature: include normal operation, cleaning, start-up, shutdown and upset conditions.
- Identify the failure mode: general corrosion, pitting, crevice corrosion, stress-corrosion cracking or intergranular attack.
- Confirm product form: bar, plate, seamless pipe, welded pipe, forging and fitting routes may use different standards.
- Review fabrication: welding, cold work, solution annealing, pickling and final surface condition can affect service performance.
- Validate the shortlist: use operating history, a materials engineer, published corrosion data or application-specific testing before final approval.
RFQ Checklist for Alloy 28 or 904L
- Grade and UNS number: N08028 or N08904.
- Product form and governing standard, including edition if the project requires it.
- Dimensions, tolerance, length, quantity and surface condition.
- Delivery and heat-treatment condition.
- MTC / EN 10204 3.1, PMI, mechanical testing, corrosion testing, UT or third-party inspection requirements.
- Service medium, concentration, temperature and destination.
Frequently Asked Questions
Is Alloy 28 the same as 904L?
No. Alloy 28 is UNS N08028 / EN 1.4563, while 904L is UNS N08904 / EN 1.4539. Their chemistry, product standards and qualified service experience differ.
What are the main alloying elements in Alloy 28?
Alloy 28 is an austenitic Fe-Ni-Cr-Mo-Cu alloy. Alleima’s nominal producer data lists approximately 27% Cr, 31% Ni, 3.5% Mo and 1.0% Cu. Acceptance should be based on the ordered standard and MTC.
What is the equivalent grade of 904L?
Common designations include UNS N08904 and EN 1.4539. “Equivalent” should not be interpreted as permission to substitute another grade without engineering approval.
Which grade is better for sulfuric acid?
There is no universal answer. 904L has extensive use in sulfuric-acid service, while Alloy 28 also performs well in strong acids. Concentration, temperature, chlorides, oxidants and contaminants must be compared with qualified corrosion data.
Which standard applies to Alloy 28 bar?
Alleima lists EN 10088-3 and EN 10272 for Sanicro 28 bar. ASTM B473 should not be used as an N08028 bar specification: its published scope did not include N08028, and ASTM withdrew B473 in 2026. State the exact product standard and edition accepted by the project.
Technical References
- Alleima: Sanicro 28 tube and pipe datasheet
- Alleima: Sanicro 28 bar datasheet
- Outokumpu: Ultra 904L product data
- ASTM B668-23: N08028 seamless pipe and tube scope
- ASTM B473-24: withdrawn scope, not an N08028 bar standard
- ASTM B649-26: current notice moving N08904 bar to A479/A484
- ASTM B677-26: current notice moving N08904 pipe and tube to A269/A312
Compare the material—or send your requirement now
Review our Alloy 28 round bar and 904L pipe product pages. For a quotation, send the grade, standard, size, quantity, service condition and inspection requirements.
Post time: Oct-08-2026