ASTM B625 Incoloy 926 UNS N08926 Plate and Sheet

Incoloy 926 plate and sheet, designated UNS N08926 / W.Nr. 1.4529, is a solution-annealed iron-nickel-chromium-molybdenum-copper-nitrogen alloy selected for chloride-bearing and mixed corrosive environments. Its elevated molybdenum and nitrogen contents support resistance to pitting, crevice corrosion and chloride-induced stress-corrosion cracking.
SASA ALLOY supplies Alloy 926 plate, sheet and cut-to-size parts to ASTM B625 / ASME SB-625 and agreed project requirements. For an accurate quotation, specify dimensions, quantity, condition, surface finish, tolerances, inspection and certificate requirements.
Product Identification and Supply Range
| Product | Alloy 926 plate, sheet, blanks, discs and profile-cut parts |
|---|---|
| Material designation | Incoloy 926 / UNS N08926 / W.Nr. 1.4529 / X1NiCrMoCuN25-20-7 |
| Primary standard | ASTM B625 / ASME SB-625 |
| Thickness | Cold rolled 1–7 mm; hot rolled 3–60 mm |
| Width and length | Width up to 2500 mm; length up to 12500 mm |
| Condition | Hot or cold rolled, solution annealed, descaled or pickled |
| Processing | Shearing, sawing, waterjet or plasma cutting, drilling and machining after drawing review |
The dimensions above describe a practical production and market supply range, not current stock. Final availability, minimum quantity and production route are confirmed for each inquiry.
Request Alloy 926 Plate Availability
Why Alloy 926 Is Selected
Approximately 6–7% molybdenum together with nitrogen supports resistance to pitting and crevice corrosion.
Chromium, nickel, molybdenum and copper provide balanced resistance in oxidizing and reducing process environments.
Plate and sheet can be cut, formed, machined and welded using procedures qualified for this high-alloy material.
Chemical Composition
| Element | Ni | Cr | Mo | Cu | N | C | Fe |
|---|---|---|---|---|---|---|---|
| Range, wt.% | 24.0–26.0 | 20.0–21.0 | 6.0–7.0 | 0.5–1.5 | 0.15–0.25 | 0.02 max | Balance |
Values are a material-identification reference. Purchase acceptance must follow the ordered standard edition and the supplied material test certificate.
Mechanical Properties in Solution-Annealed Condition
| Property | Reference value for sheet/plate ≤50 mm | Purchasing note |
|---|---|---|
| 0.2% yield strength | 300 MPa minimum | Confirm ordered standard and thickness |
| Tensile strength | 600–800 MPa | Verify supplied heat on the MTC |
| Elongation | 40% minimum | Specimen orientation and thickness rules apply |
These are manufacturer reference values for solution-annealed material, not a test certificate for every plate. Contract acceptance values must be stated in the purchase order.
Surface, Cutting and Fabrication
- Surface: hot-rolled plate can be solution annealed and descaled or pickled; cold-rolled sheet can be supplied with the agreed mill or processed finish.
- Cut-to-size: rectangular blanks, discs and profile-cut parts can be reviewed from drawings.
- Forming: the alloy work-hardens; forming sequence, bend radius and rolling direction should be defined before production.
- Machining: rigid equipment, positive tooling, controlled cutting parameters and adequate coolant are recommended.
- Welding: use a qualified procedure and compatible filler metal selected for the service environment.
Inspection, Testing and Documentation
- Material test certificate with heat number, chemical analysis and mechanical-property traceability.
- Dimensional and visual inspection for thickness, width, length, flatness and surface condition.
- PMI, ultrasonic testing, third-party inspection or additional corrosion testing when specified in the order.
- EN 10204 3.1 certificate or another agreed documentation format when requested.
Additional testing requires a defined method, sampling plan and acceptance criterion. Product photographs illustrate the plate form; grade identity is established by traceability, the MTC and agreed inspection.
Typical Applications and Selection Factors
Alloy 926 plate and sheet are considered for seawater and offshore systems, flue-gas desulfurization equipment, phosphoric and sulfuric acid service, salt concentration and crystallization equipment, heat exchangers, chemical tanks, pulp bleaching equipment and cooling-water systems.
Final selection should consider chloride level, acid concentration, temperature, pressure, contaminants, aeration, crevice geometry, fabrication condition and cleaning method. Include service conditions when material-selection review is required.
Ordering Checklist
- Material: Alloy 926 / UNS N08926 / W.Nr. 1.4529
- Standard and required edition: ASTM B625 or ASME SB-625
- Product form: plate, sheet, blank, disc or cut part
- Thickness × width × length and quantity
- Condition, surface finish, flatness and dimensional tolerances
- Cutting, forming or machining allowance
- Required MTC, inspection, testing and third-party witnessing
- Marking, packing, destination and project documentation requirements
Frequently Asked Questions
What standard covers Incoloy 926 plate and sheet?
ASTM B625 covers UNS N08926 plate, sheet and strip in the annealed condition. The required edition and any ASME adoption should be stated in the purchase order.
What is the difference between Alloy 926 and Alloy 825 plate?
Alloy 926 contains substantially more molybdenum together with nitrogen, giving stronger resistance to localized corrosion in aggressive chloride environments. The correct choice still depends on the actual process medium and temperature.
Can UNS N08926 plate be supplied as custom-cut parts?
Yes. Blanks, discs and profile-cut pieces can be reviewed. Send a drawing with dimensions, tolerances, edge condition, quantity and inspection requirements.
Do plate photographs confirm the N08926 grade?
No. Photographs show the product form only. Grade confirmation requires heat-number traceability, the material test certificate and any ordered PMI or third-party inspection.
Request an Alloy 926 Plate Quotation
Send the ASTM B625 / UNS N08926 requirement with size, quantity, condition, surface, tolerance, testing and certificate details. We will review the specification and production route before quotation.